NICKEL GUARD SP:PROTECTIVE AGENT FOR Ni PLATING
This is for electroless Ni plating and prevent development rust for next process.
Treatment is just dipping in room temperature.
Treatment is just dipping in room temperature.
Characteristic
- Does not contain any chromium compounds
- Not PRTR applicable
- Treatment process is simple due to the dipping treatment, making it easy to work with
Performance
The Effects of Chromic Acid and Similar Corrosion Resistance
Salt spray test - 4 hours (electroless nickel 3μm: P10% on top of iron)
Salt spray test - 4 hours (electroless nickel 3μm: P10% on top of iron)
Process
Electroless Ni plating → Washing → NICKEL GUARD SP → Rinsing → Dry
Working condition
- Concentration =5~10% (Dilute by water)
- Temperature = Room temperature (20~35℃)
- Dipping time = 1minute (More than 1 minute)
- PH = 7~9 (Operate neutrality or alkalinity)
- Stirring = Lightly
- Material of tank = Plastic (Polyethylene, Polypropylene, PVC etc.) SUS