FC-X Series:For Nickel allergy(Nonmagnetism)Non Cyanide Copper-Tin alloy plating
The most process for Nickel allergy was used cyanide before.
This Copper-Tin alloy process is not used cyanide and the process of the neutral of the nickel substitution plating.
This Copper-Tin alloy process is not used cyanide and the process of the neutral of the nickel substitution plating.
Characteristic
-
It does not use the cyanide
- Not necessity to control such as poison
- Easy to control as waste water treatment
- Low risk for working condition
- Same appearance and corrosion resistance with Ni
-
It have two types of for barrel plating and racking plating
It is possible to get 5 microns by racking plating
-
Application
- For clothes such as hook, fastener etc.
- Accessories such as necklace etc.
- Glasses
- Housing, button for such as mobile phone, digital camera
-
Application
- Temperature: 25℃, 75°F (20-30℃, 70-85°F)
- pH: 7 (6.0-7.0)
- Current density: 1A/dm2 (0.5-1.5A/dm2)
- Anode: Carbon plate *Anode: cathode = 2+:1
- Plating speed: Approx. 2 microns/5 min *1A/dm2
- Mixing: Gentle liquid circulation filtration
- Plating tank: PVC, PE, FRP